3M 850

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 850

Main features

  • Low-Caliper High-Strength Process Tape
  • Quick-Stick Long-Hold Splicing
  • Visible or Transparent Marking Options

Product Description

3M Polyester Film Tape 850 is a thin polyester film tape with acrylic pressure-sensitive adhesive for splicing, marking, label protection, masking, and process protection. Its high-strength polyester backing meets low-caliper requirements so the tape can pass through many machinery processes while resisting tearing, abrasion, and rough handling. The acrylic adhesive provides quick stick and long-term holding in splicing applications. Transparent and colored versions are available for different process needs: transparent material provides chemical and solvent resistance, while colored versions improve visibility for marking or identification. The construction is suited to web handling and other operations that require a thin, durable film tape.

Key features

  • Low-caliper polyester film: The thin, high-strength backing limits added bulk while resisting tearing and abrasion during machinery and web processes.
  • Quick-stick acrylic adhesion: The pressure-sensitive acrylic adhesive provides fast tack and long-term holding for splicing applications.
  • Version-specific process options: Transparent material adds chemical and solvent resistance, while colored versions increase visibility for marking and identification.

Applications

Use 3M Polyester Film Tape 850 for film and paper splicing, web processing, label protection, decorative edging, masking, surface protection, marking, and electrical or electronic process work.

Technical Specifications

General Properties
Color
The color
Transparent, Red, Black, White
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
120 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
49 N/cm
Other Properties
Storage Temperature
16 - 27 °C