3M 847

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 847

Main features

  • Medium-Viscosity Application Control
  • Fuel and Oil Resistance
  • Adhesion-Promoting Surface Treatment

Product Description

3M™ Nitrile High Performance Rubber & Gasket Adhesive 847 is a medium-viscosity, quick-drying adhesive designed for brush or flow applications. It forms strong, flexible bonds and exhibits excellent resistance to many fuels and oils, ensuring long-lasting durability. This adhesive is highly effective for bonding leather, nitrile rubber, most plastics, and gasketing materials to a variety of substrates, and it can be heat cured to achieve improved physical properties.

Key features

  • Quick drying and flexible: Rapidly forms strong, flexible bonds for efficient assembly and lasting performance.
  • Fuel and oil resistance: Delivers excellent durability and resistance to many fuels and oils in demanding environments.
  • Heat curable: May be heat cured to obtain improved physical and mechanical properties.

Applications / Suitable for

  • Bonding leather and nitrile rubber
  • Adhering most plastics and gasketing materials to a variety of substrates
  • Medium-viscosity brush or flow applications

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Dark Brown
Chemistry Type
Nitrile Rubber
Solids
46 — 55 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-18 °C
Mechanical Properties
Peel Strength
1.6 N/cm
Physical Properties
Net Weight
75 - 79 kg/m3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Nitrile Rubber - -
Color Dark Brown - -
Solids Content by Weight 46-55 % -
Net Weight 7.5-7.9 lb/gal -
Carrier Solvent Acetone - -
Viscosity 5,000-90,000 cP at 27°C (80°F)
Flash Point -18 °C (0°F) Closed Cup
Bonding Range Up to 10 minutes 10 mil wet film 2 surfaces
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
180° Peel Adhesion 376 oz/in Canvas to Steel, 72 h at 23°C (73°F)
180° Peel Adhesion 640 oz/in Canvas to Steel, 3 week at 23°C (73°F)
Overlap Shear Strength 152 lb/in² Birch to Birch, 3 week cure, tested at 1°C (30°F)
Overlap Shear Strength 20 lb/in² Birch to Birch, 3 week cure, tested at 66°C (150°F)

Leading Brands Trust in Our Products and Services