3M 76

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M 76

Main features

  • High-Tack Industrial Formulation Excels in One-Surface Bonding
  • Polyethylene and Polypropylene Bonding
  • Controlled Variable Lace Spray Pattern

Product Description

3M™ Hi-Tack 76 Spray Adhesive is an industrial aerosol spray adhesive formulated with high tack for single-surface bonding applications. This translucent, synthetic elastomer-based adhesive effectively bonds hard-to-hold materials such as polyethylene and polypropylene. It provides a variable lace spray pattern and is an excellent choice for adhering fabric headliners, rubber, felt, plastics, and foil to themselves or to wood and metal surfaces.

Key features

  • High-tack performance: Formulated specifically for efficient one-surface bonding applications with a rapid 1-2 minute dry time.
  • Bonds difficult substrates: Effectively adheres to hard-to-hold plastics, including polyethylene and polypropylene.
  • Variable lace spray: Aerosol delivery provides a controlled variable lace pattern for precise application and a coverage of up to 2.6 m² (28 ft²) per can.

Applications / Suitable for

  • One-surface bonding applications
  • Bonding polyethylene and polypropylene plastics
  • Attaching fabric headliners
  • Bonding rubber, felt, cardboard, cork, and foil to wood or metal

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Translucent
Chemistry Type
Synthetic Elastomer
Density (g)
0.78 g/cm3
Solids
13.5 %
Physical Properties
Dry Time
1-2 minutes
VOC
<55
Thermal Properties
Shear Adhesion Failure Test - SAFT
110 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Synthetic Elastomer - -
Color Translucent - -
Spray Pattern Variable Lace - -
Solids Content by Weight 13.5 % -
Density 0.78 kg/L (6.5 lb/gal)
Coverage 2.6 m² (28 ft²) at 27 g/m² dry
Dry Time 1-2 minutes Dependent on ambient conditions and coverage
Bonding Range 1-10 minutes 1 surface
Bonding Range 1-60 minutes 2 surfaces
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Shear Adhesion Failure Test (SAFT) 110 °C 230°F (birch plywood, 25 mm overlap, 100 g)

Leading Brands Trust in Our Products and Services