3M 69

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 69

Main features

  • High-Temperature Electrical Insulation
  • Glass-Cloth Coil and Motor Wrapping
  • No-Heat Adhesive Application

Product Description

3M Glass Cloth Electrical Tape 69 is a white, 0.178 mm electrical insulation tape with a glass-cloth backing and a non-corrosive, flame-retardant, thermosetting silicone pressure-sensitive adhesive. The adhesive applies without heat or moisture preparation, while the glass-cloth construction provides a defined tape format for high-temperature electrical assembly. The tape is designed for continuous operation not exceeding 200 deg C under its UL listing and 180 deg C under its CSA listing. Its electrical and mechanical properties suit insulation, splicing, bundling, and coil-wrapping applications where a glass-cloth tape is specified.

Key features

  • High-temperature electrical insulation: The tape is rated for continuous operation up to 200 deg C under UL and 180 deg C under CSA.
  • Glass-cloth silicone construction: A 0.140 mm glass-cloth backing with thermosetting silicone adhesive provides a 0.178 mm insulation tape.
  • Ready pressure-sensitive application: The adhesive applies without heat or moisture preparation for coil, transformer, and motor assembly.

Applications

It is used for coil, transformer, and motor insulation, lead anchoring, high-temperature electrical splicing, and bundling.

Product Family

3M 69

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
177 μm
Other Properties
Storage Temperature
10 - 27 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
5 %
Thermal Properties
Operating Temperature
200 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhiteVisual
Backing materialGlass clothAs supplied
Backing thickness0.140mmNominal
Total thickness0.178 +/- 0.025mmASTM D1000; 23 deg C
AdhesiveThermosetting siliconePressure-sensitive
Breaking strength>= 263N/cmMinimum; ASTM D1000; 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Dielectric breakdown>= 2000VMinimum; ASTM D1000; 23 deg C
Insulation resistance>= 50 x 10^6ohmMinimum; ASTM D1000 high-humidity method
Adhesion to steel>= 3.3N/cmMinimum; ASTM D1000; 23 deg C
UL continuous operating temperature200deg CDo not exceed; UL listing
CSA continuous operating temperature180deg CDo not exceed; CSA listing