3M 604NS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 604NS

Main features

  • Non-Sag Vertical Gap Filling
  • Rapid 4-Minute Working Window
  • Multi-Material Structural Bonding

Product Description

3M Scotch-Weld Urethane Adhesive 604NS is a two-part, non-sag polyurethane adhesive for structural and semi-structural bonding where gap filling and vertical or overhead application are important. In the DP604NS Duo-Pak configuration, the 1:1 components dispense as a bubble-free non-sag paste with a typical 4-minute work life, 20-minute tack-free time, and 6-hour full cure at 25 deg C. The adhesive is used with concrete, ceramic, wood, glass, metals, plastics, and rubber in construction, maintenance, and assembly work. Its rapid setting profile and sag resistance suit bonded joints that must stay in place during cure.

Key features

  • Non-sag gap filling: The mixed adhesive stays as a non-sag paste for vertical and overhead bonding while filling joint gaps.
  • Rapid working and cure: DP604NS has a typical 4-minute work life, 20-minute tack-free time, and 6-hour full cure at 25 deg C.
  • Multi-material structural bonding: The adhesive is used with concrete, ceramic, wood, glass, metals, plastics, and rubber in construction and assembly work.

Applications

Applications include structural and semi-structural bonding of concrete, ceramic, wood, plastics, rubber, metals, glass, and selected construction assemblies.

Technical Specifications

General Properties
Color
The color
Black
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
4 minutes
Thermal Properties
Operating Temperature
-51 to 121 °C

Additional Information

Technical properties

As-supplied / before-processing properties

DP604NS black Duo-Pak configuration; component data are shown at the stated conditions.

PropertyValueUnitMethod / condition
Part A viscosity1493cPTypical; HBDVI + CP, 25 deg C
Part B viscosity1237cPTypical; HBDVI + CP, 25 deg C
Mix ratio1:1DP604NS Duo-Pak components
Shelf life6monthsUnopened package; 18 to 30 deg C
Technical properties

After-processing / final-state properties

DP604NS black data; final properties apply under the stated cure and test conditions.

PropertyValueUnitMethod / condition
Hardness85Shore ATypical; ASTM D2240-91; after full cure
Lap shear strength900psiTypical; ASTM D1002-72; 7 days at 25 deg C
Continuous temperature range-51 to 121deg CTypical; PEC