3M 5952

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 5952

Main features

  • 45-Mil Conformable Foam Bonding
  • Painted-Surface Permanent Attachment
  • Panel and Display Assembly Bonding

Product Description

3M VHB Tape 5952 is a black, double-sided modified acrylic foam bonding tape with a 45 mil nominal thickness for permanent attachment to painted and powder-coated surfaces. Its conformable acrylic foam core is paired with modified acrylic adhesive on both sides and a release liner for pre-application handling. The continuous foam-tape construction is used to join panels, trim, stiffeners, displays, and frames where a conformable permanent bond is required. The product is supplied in multiple widths, lengths, and converted formats for configuration-specific industrial assembly needs.

Key features

  • 45 mil foam construction: The black double-sided tape combines 45 mil nominal thickness with a conformable acrylic foam core.
  • Painted-surface attachment: Modified acrylic adhesive supports permanent bonding to documented painted and powder-coated surfaces.
  • Panel and display assembly: The tape is used to join panels, trim, stiffeners, displays, and frames in documented assemblies.

Applications

Applications include permanent bonding of panels, trim, stiffeners, displays, and frames to documented painted and powder-coated surfaces.

Product Family

3M 5952

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Modified Acrylic
Color
The color
Black
Density
Volumetric mass per unit
590 kg/m3
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
PE Film
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1100 μm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBlackTape body
Adhesive typeModified acrylicBoth sides
CoreConformable acrylic foamDouble-sided construction
Nominal tape thickness45milProduct type record
Release linerPresentLinered construction