3M 5925

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 5925

Main features

  • Immediate Painted-Surface Bonding
  • Conformable 0.6 mm Foam Attachment
  • 93 deg C Long-Term Use

Product Description

3M VHB Tape 5925 is a black, double-sided modified acrylic foam tape for permanent attachment on painted and powder-coated surfaces. Its conformable foam core and modified acrylic adhesive provide a 0.6 mm applied thickness and immediate handling strength without a curing step. The tape combines high shear strength, conformability, and surface adhesion and is rated for long-term use up to 93 deg C. It is used for trim, nameplates, electronic displays, panel-to-frame and stiffener-to-panel bonding, with documented adhesion to materials including stainless steel and other compatible surfaces.

Key features

  • Immediate painted-surface handling: The modified acrylic construction bonds many painted and powder-coated surfaces with immediate handling strength and no cure wait.
  • Conformable 0.6 mm foam: The foam core provides a 0.6 mm applied bonding layer that conforms across the joined surfaces.
  • Long-term 93 deg C use: The tape is rated for long-term use at temperatures up to 93 deg C.

Applications

Applications include bonding trim, nameplates, electronic displays, panels, frames, and stiffeners, including permanent attachment to painted and powder-coated surfaces.

Product Family

3M 5925

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Modified Acrylic
Color
The color
Black
Density
Volumetric mass per unit
590 kg/m3
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
PE Film
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
600 μm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBlackTape body
Adhesive typeModified acrylicBoth sides
CoreConformable acrylic foamDouble-sided construction
Total tape thickness0.6mm25 mil; applied tape
Liner materialPolyethylene filmRelease liner

Leading Brands Trust in Our Products and Services