Main features

  • One-Part Moisture-Cure Joint Sealing
  • Elastic >600% Elongation Profile
  • 60 to 90 Minute Tack-Free Window

Product Description

3M Polyurethane Sealant 540 is a one-component, moisture-curing polyurethane sealant that forms a permanent elastic bond for construction and industrial joints. The medium-paste material reaches tack-free condition in 60 to 90 minutes and cures at a typical rate of 3 mm per 24 hours. After cure, it has a Shore A hardness of 40, tensile strength of 2.1 MPa, and elongation at break above 600%. The sealant bonds documented materials including plastics, metals, fiberglass, and wood and is used in expansion joints, masonry joints, curtain walls, doors, windows, lap seams, and compatible submerged applications.

Key features

  • One-component moisture cure: The medium-paste sealant requires no component mixing and reaches tack-free condition in 60 to 90 minutes.
  • Elastic cured profile: Typical cured properties include Shore A 40 hardness and elongation at break above 600%.
  • Construction joint versatility: The sealant bonds documented plastics, metals, fiberglass, and wood for multiple joint and seam applications.

Applications

Applications include expansion and control joints, precast and tilt-up construction, masonry joints, curtain walls, doors and windows, lap seams, and compatible submerged applications.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
medium paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.17
Physical Properties
Tack-Free Time
60-90 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
600 %
Thermal Properties
Operating Temperature
5-35 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ConsistencyMedium pasteTypical uncured property
Specific gravity1.17Typical physical property
SaggingNoneISO 7390; typical
VOC53.7g/LTypical physical property
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore A hardness40ASTM C661; typical cured characteristic
Modulus at 100% elongation0.9MPaASTM D412; typical cured characteristic
Tensile strength2.1MPaASTM D412; typical
Elongation at break>600%ASTM D412; typical
Long-term temperature resistance-40 to 90deg CTypical; continuous exposure above 90 deg C decreases tensile strength over time