3M 50

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M 50

Main features

  • All-Weather Pipe Corrosion Protection
  • Conformable High-Tack Pipe Wrapping
  • Primer-Controlled Metal Surface Adhesion

Product Description

3M Scotchrap Vinyl Corrosion Protection Tape 50 is a black, 10 mil PVC corrosion-protection tape with a high-tack pressure-sensitive rubber adhesive for wrapping metal piping systems, conduits, fittings, and field joints. The flexible construction combines conformability with electrical insulation and resistance to corrosion, impact, abrasion, puncture, weathering, and common chemical exposure. Its normal service temperature range is -48 to 80 deg C. Metal surfaces must be clean and prepared with 3M Scotchrap Pipe Primer before wrapping to establish the documented application system.

Key features

  • Flexible PVC corrosion barrier: The 10 mil PVC backing conforms around pipes, conduits, fittings, and field joints while providing mechanical protection.
  • High-tack rubber adhesive: Pressure-sensitive rubber adhesive supports secure wrapping on prepared metal surfaces above and below ground.
  • Primer-controlled installation: All metal surfaces require 3M Scotchrap Pipe Primer before the tape is wrapped for the documented corrosion-protection system.

Applications

Suitable uses include corrosion protection of metal pipes, conduits, fittings, joints, and mill-coated pipe systems in electrical and utility maintenance.

Technical Specifications

Other Properties
Storage Temperature
10 - 27 °C
General Properties
Color
The color
Black
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
100 %
Thermal Properties
Temperature Range
-48 to 80 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Backing materialPolyvinyl chloride (PVC)Flexible tape backing
Adhesive typeRubberPressure-sensitive
ColorBlackBacking and adhesive
Total tape thickness0.254mm10 mil; typical; Tape 50
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion to steel0.219kN/mASTM D1000; 23 deg C; typical
Water vapor transmission rate1.0g/100 in^2/24 hASTM D3833; typical
Moisture absorption0.30%ASTM D570; typical
Dielectric breakdown voltage12000VASTM D1000 unless otherwise stated; typical
Normal service temperature range-48 to 80deg CTypical; installed tape

Leading Brands Trust in Our Products and Services