3M 4950

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4950

Main features

  • Immediate No-Cure Assembly Handling
  • Firm 1.1 mm Foam Bonding
  • High-Surface-Energy Permanent Attachment

Product Description

3M VHB Tape 4950 is a white, double-sided acrylic foam tape for permanent bonding of metals, glass, and other high-surface-energy materials. A firm acrylic foam core with general-purpose acrylic adhesive provides a 1.1 mm tape thickness and immediate handling strength without a fixturing or cure wait. The tape is rated for long-term use up to 93 deg C and short-term exposure up to 149 deg C for up to four hours. Its permanent bonding format is used for stiffener-to-panel and panel-to-frame attachment, decorative trim, nameplates, and logos.

Key features

  • Immediate no-cure handling: Pressure-sensitive all-acrylic bonding develops immediate handling strength without a fixturing or cure wait.
  • Firm 1.1 mm foam core: The firm acrylic foam construction provides a 1.1 mm double-sided bonding layer for permanent attachment.
  • High-surface-energy bonding: General-purpose acrylic adhesive bonds metals, glass, and other documented high-surface-energy substrates.

Applications

Applications include stiffener-to-panel bonding, panel-to-frame attachment, decorative trim, nameplates, and logos.

Technical Specifications

General Properties
Color
The color
White
Density
Volumetric mass per unit
800 kg/m3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
1100 μm
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhiteTape body
Adhesive typeGeneral-purpose acrylicBoth sides
CoreFirm acrylic foamDouble-sided construction
Total tape thickness1.1mm45 mil; product thickness
Liner materialDensified kraft paperRelease liner