3M 4905

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4905

Main features

  • Low-Visibility Permanent Fastening
  • Immediate Contact-Bond Handling
  • High-Strength HSE Substrate Bonding

Product Description

3M VHB Tape 4905 is a clear, double-coated solid acrylic tape for permanent bonding where a low-visibility fastening method is preferred. The 0.5 mm construction uses general-purpose acrylic adhesive on both sides with a red printed PE film liner. It bonds on contact to provide immediate handling strength and is intended for high-surface-energy substrates including metals, glass, polycarbonate, and acrylic. The tape can replace rivets, welds, screws, or liquid adhesives in transparent assemblies, signage, decorative trim, nameplates, and panel attachments while keeping bonded surfaces smooth.

Key features

  • Clear permanent fastening: The transparent acrylic construction keeps bonded surfaces smooth and visually unobtrusive.
  • Immediate contact handling: Pressure-sensitive adhesive bonds on contact without waiting for a cure cycle.
  • Strong HSE attachment: Typical 21 N/cm peel adhesion and 480 kPa overlap shear on stainless steel quantify attachment to high-surface-energy designs.

Applications

Applications include joining transparent materials, mounting backlit signs, edge-bonding resin-filled glass, decorative trim, nameplates, logos, and panel-to-frame attachment.

Technical Specifications

General Properties
Color
The color
Clear | Red (printed)
Density
Volumetric mass per unit
960 kg/m3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
500 μm
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorClearTape body
Adhesive typeGeneral-purpose acrylicBoth sides
Total tape thickness0.5mmASTM D3652; typical
Thickness tolerance+/-15%Typical
Density960kg/m^3ASTM D3574; typical
LinerRed printed PE film0.13 mm thickness
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
90 deg peel adhesion21N/cmASTM D3330; stainless steel; 23 deg C; 72 h dwell; 5 mil aluminum foil backing; 300 mm/min; typical
Normal tensile690kPaASTM D897; aluminum; 23 deg C; 72 h dwell; 6.45 cm^2; 51 mm/min; typical
Overlap shear strength480kPaASTM D1002 and ISO 4587; stainless steel; 23 deg C; 72 h dwell; 6.45 cm^2; 12.7 mm/min; typical
Short-term temperature resistance149deg C4 h conditioning; 100 g static load; no change in room-temperature dynamic shear; typical
Long-term temperature resistance93deg CASTM D3654; stainless steel; 500 g; 6.5 cm^2; 10,000 minutes; typical

Leading Brands Trust in Our Products and Services