3M 471

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 471

Main features

  • Conformable Irregular-Surface Marking
  • Clean-Removal Paint Masking
  • Vivid Abrasion-Resistant Identification

Product Description

3M Vinyl Tape 471 is a conformable colored vinyl tape with rubber adhesive for lane and safety marking, color coding, paint masking, sealing, and temporary surface protection. The 0.14 mm tape stretches around curved, convex, and irregular surfaces while retaining its applied shape. Pigmented backings maintain vivid color under heavy abrasion, and the tape removes cleanly from many surfaces. Good solvent resistance and a choice of seven colors support plant marking and general process use. Apply the tape to clean, dry surfaces at 16 to 27 deg C for best results.

Key features

  • Conformable dead stretch: The vinyl backing follows curved and irregular surfaces without lifting or retracting.
  • Clean surface removal: Rubber adhesive provides immediate holding strength and clean removal from many surfaces.
  • Abrasion-resistant color: Pigmented backings retain vivid identification colors under heavy abrasion.

Applications

Applications include lane and safety marking, color coding, fine-line paint masking, temporary surface protection, container sealing, bundling, and decorating.

Technical Specifications

General Properties
Color
The color
Yellow, white, red, black, green, orange, blue
Other Properties
Storage Temperature
16 - 27 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
130 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
24.5 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorYellow, white, red, black, green, orange, bluePigmented backing
Adhesive typeRubberPressure-sensitive
Backing thickness0.1mmASTM D3652; typical
Total tape thickness0.14mmASTM D3652; typical
Shelf life18monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH; out of direct sunlight
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion2.5N/cmASTM D3330; 23 deg C; 300 mm/min; typical
Elongation at break130%ASTM D3759; typical
Tensile strength24.5N/cmASTM D3759; typical
Long-term temperature resistance77deg CDays to weeks; typical
Minimum long-term temperature resistance4deg CDays to weeks; typical