3M 470L

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 470L

Main features

  • Linered Die-Cut Plating Masks
  • Chemical-Resistant Process Protection
  • Conformable Curved-Surface Masking

Product Description

3M Electroplating Tape 470L is the linered configuration of a tan vinyl electroplating tape, pairing a conformable backing with rubber pressure-sensitive adhesive for die-cut masks and chemical-process protection. Its 0.18 mm overall thickness, release liner, and flexible construction support conversion into shaped masks for curved or irregular parts. The tape resists most chemicals used in typical electroplating and anodizing operations and most common solvents. It also accepts marker ink and thermal-transfer printing for identification during electroplating, anodizing, milling, etching, peening, coated-rack protection, and labeling.

Key features

  • Linered conversion format: The release liner supports die-cutting and handling of shaped electroplating masks.
  • Chemical-process resistance: The tape resists most chemicals used in typical electroplating and anodizing operations.
  • Conformable vinyl backing: Flexible construction follows curved and irregular surfaces during masking and protection.

Applications

Applications include die-cut electroplating and anodizing masks, coated-rack protection, milling, etching, peening, labeling, and sealing containers from water intrusion.

Product Family

3M 470L

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Tan
Other Properties
Storage Temperature
16 - 27 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
180 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
35 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorTanTape body
Adhesive typeRubberPressure-sensitive
Backing materialVinylLinered configuration
Backing thickness0.16mm6.3 mil; typical
Overall thickness0.18mm7.1 mil; tape excluding liner
Shelf life18monthsAs supplied
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Adhesion strength4N/cm
Elongation at break180%
Tensile strength35N/100 mm