3M 470

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 470

Main features

  • Chemical-Resistant Plating Masks
  • Conformable Irregular-Surface Coverage
  • Clean-Removal Process Masking

Product Description

3M Electroplating Tape 470 is an unlined, tan vinyl tape with a rubber pressure-sensitive adhesive for masking in electroplating, anodizing, milling, etching, and peening operations. The 0.18 mm tape combines a conformable, abrasion-resistant backing with resistance to most chemicals used in typical electroplating processes and to most common solvents. It follows curved or irregular surfaces and removes cleanly from most surfaces after use. Ketones, chlorinated hydrocarbons, and esters can swell or curl the backing. The printable surface accepts marker ink and thermal-transfer printing for identification during processing.

Key features

  • Electroplating chemical resistance: The vinyl construction resists most chemicals used in typical electroplating and anodizing operations.
  • Conformable process masking: Flexible backing covers curved and irregular surfaces during plating, milling, etching, and peening.
  • Printable clean removal: The marking surface accepts ink and thermal-transfer printing, then removes cleanly from most surfaces.

Applications

Applications include flat-strip and overlapping electroplating masks, anodizing masks, coated-rack protection, milling, etching, peening, labeling, and container sealing.

Technical Specifications

General Properties
Color
The color
Tan
Other Properties
Storage Temperature
16 - 27 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
180 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
35 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorTanTypical
Adhesive typeRubberPressure-sensitive
Backing materialVinylUnlined configuration
Backing thickness0.16mmASTM D3652; typical
Total tape thickness0.18mmASTM D3652; typical
Shelf life18monthsOriginal packaging; 16 to 27 deg C and 40 to 60% RH; out of direct sunlight
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion4N/cmASTM D3330; 23 deg C; 304 mm/min; typical
Elongation at break180%ASTM D3759; typical
Tensile strength35N/cmASTM D3759; typical
Long-term temperature resistance121deg CDays to weeks; typical

Leading Brands Trust in Our Products and Services