3M 444

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 444

Main features

  • Fast Initial Lamination Adhesion
  • Stable PET Converting Carrier
  • Foam and Gasket Attachment

Product Description

3M Double Coated Tape 444 is a pressure-sensitive laminating tape built with 3M Adhesive 300 on both sides of a 0.5 mil PET film carrier and a densified kraft release liner. The medium-firm acrylic adhesive delivers high initial adhesion to foams, fabrics, coated papers, polyethylene, and other high- and low-surface-energy plastics. Its film carrier adds dimensional stability for slitting and die-cutting, while different adhesive thicknesses on the two faces promote wet-out during assembly. The tape is used for foam lamination, gasket attachment, plastic-film bonding, splicing, and diagnostic test-strip assembly.

Key features

  • Rapid lamination adhesion: Quick-flowing 3M Adhesive 300 develops high initial adhesion for efficient laminating.
  • Stable converting carrier: A 0.5 mil PET film improves handling and dimensional stability during slitting and die-cutting.
  • Low-surface-energy attachment: The acrylic adhesive bonds foams and plastics such as polyethylene for gasket and laminate assembly.

Applications

Applications include foam lamination, gasket attachment, plastic-film bonding, splicing, and medical diagnostic test-strip assembly.

Technical Specifications

General Properties
Adhesive Thickness
Adhesive thickness indicates the thickness of an adhesive layer. It refers to the adhesive thickness of a single side so for double sided tapes it always needs to be multiplied.
50.8 µm
Color
The color
White
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Tape caliper3.9milTypical product construction
Carrier materialPET filmDouble-coated carrier
Carrier thickness0.5milPET film
Face-side adhesive thickness2mil3M Adhesive 300
Liner-side adhesive thickness1.4mil3M Adhesive 300
Release liner55# densified kraft3.2 mil caliper

Leading Brands Trust in Our Products and Services