3M 4298UV

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4298UV

Main features

  • Fast 30-to-90-Second Drying
  • Fluorescent Coverage Verification
  • Multiple Application Methods

Product Description

3M Adhesion Promoter 4298UV is a fast-drying liquid primer that improves the adhesion of 3M Acrylic Foam Tape and 3M Acrylic Plus Tape to low- and medium-surface-energy plastics used in automotive trim and parts. At a recommended wet coating thickness of approximately 0.002 inch (0.05 mm) or less, the promoter typically dries in 30 to 90 seconds. A fluorescent dye makes the applied coating visible for coverage verification. It can be applied by gravity-feed wipe, knurled roller, sprayer, felt-tipped applicator, or a similar method. Applications include tape-bond surface preparation for TPO, TPU, polypropylene, EPDM, polycarbonate, acrylic, ABS, nylon, glass, TPV, and TPE.

Key features

  • Rapid Drying: Dries in a typical 30 to 90 seconds at approximately 0.002 inch wet coating thickness, with time dependent on temperature and humidity.
  • Visible Coverage Check: Fluorescent dye makes the applied promoter visible for coverage verification.
  • Flexible Application Methods: Can be applied by gravity-feed wipe, knurled roller, sprayer, felt-tipped applicator, or a similar method.

Applications

Suitable for preparing specified automotive plastics and trim materials before applying compatible 3M Acrylic Foam Tape or 3M Acrylic Plus Tape.

Technical Specifications

General Properties
Color
The color
Yellow
Physical Properties
Drying Time
30-90 seconds
Net Weight
820 kg/m3
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
25 mPa.s
Other Properties
Storage Temperature
4 - 38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorYellow-As supplied
Viscosity<=25cPMaximum
Drying time30 to 90secondsTypical at approx. 0.002 in (0.05 mm) wet coating; varies with temperature and humidity
Coverage75 (800)m^2/gal (ft^2/gal)Based on 0.002 in wet coating thickness
Net weight820 (6.8)g/L (lb/gal)As supplied
Recommended wet coating thickness<=0.002 (0.05)in (mm)Apply a thin, uniform coating
Tape application window<=1hourAfter promoter application; keep the primed surface free of contaminants