3M 427

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 427

Main features

  • Dead-Soft Aluminum Foil Backing
  • Moisture-Barrier Tape Applications
  • -54 to 149 deg C Temperature Resistance

Product Description

3M™ Aluminum Foil Tape 427 combines a nominal 3 mil dead-soft aluminum foil backing with a transparent acrylic adhesive and an easy-release paper liner. The tape provides a conformable metallic surface for industrial masking, holding, patching, sealing, splicing, and heat-reflective applications. Its low water-vapor transmission rate supports moisture-barrier uses, while the aluminum backing reflects heat and light. The tape is flame resistant, meets the requirements of FAR 25.853(a), and carries documented UL 746C and UL 723 Class “L” ratings.

Key features

  • Conformable foil construction: Dead-soft aluminum backing conforms to surfaces for masking, holding, patching, sealing, and foil-splicing applications.
  • Moisture and temperature performance: Provides a typical water-vapor transmission rate of 0.77 g/m²/24 h and long-term temperature resistance from -54°C to 149°C.
  • Documented flame-performance requirements: Meets FAR 25.853(a), UL 746C, and UL 723 Class “L” requirements and can be certified to meet L-T-80C.

Applications / Suitable for

  • Aircraft paint-stripping masking
  • Moisture barriers in white-goods appliances
  • General-purpose heat reflection and heat dissipation
  • Holding wires and cooling coils in white-goods appliances
  • Repairing tears on truck trailers and aircraft
  • Splicing thin-gauge foils
  • Indoor and outdoor holding, patching, and sealing
Product Family

3M 427

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
Acrylic
Basis Weight
Basis weight refers to the weight measured in pounds off 500 sheets of paper in that paper’s basic sheet size.
5.54 g/m2
Color
The color
Shiny Silver
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.07 mm
Release Liner
A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Easy release paper
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
120 μm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
6 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical construction and physical properties of 3M™ Aluminum Foil Tape 427 as supplied. Values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
Color Shiny silver — Typical
Backing Dead-soft aluminum — Typical construction
Adhesive type Acrylic — Transparent adhesive
Backing thickness 0.07 (2.8) mm (mil) ASTM D3652
Total tape thickness 0.12 (4.6) mm (mil) ASTM D3652; liner excluded
Liner Easy-release paper — 0.08 mm (3.1 mil) liner thickness
Approximate weight 5.54 (0.012) g/m/24 mm (lb/yd/in) Typical
Technical properties

After-processing / final-state properties

Typical performance characteristics of 3M™ Aluminum Foil Tape 427. Values are representative and are not intended for specification purposes.

Property Value Unit Method / condition
180° peel adhesion 5.5 (50) N/cm (oz/in) ASTM D3330; 23°C (73°F); 304 mm/min (12 in/min)
Tensile strength 49 (28) N/cm (lb/in) ASTM D3759
Elongation at break 6 % ASTM D3759
Water-vapor transmission 0.77 (0.05) g/m²/24 h (g/100 in²/24 h) ASTM D3833
Long-term temperature resistance -54 to 149 (-65 to 300) °C (°F) Long-term exposure defined as days or weeks

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers