3M 4200FC

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4200FC

Main features

  • Fast Moisture-Cure Sealing
  • Non-Sag Marine Application
  • Flexible Bonds for Disassembly

Product Description

3M Marine Adhesive Sealant Fast Cure 4200FC is a one-part, moisture-curing polyurethane paste for bonding and sealing marine joints and hardware. Its medium-strength elastomeric seal is watertight and weather resistant while allowing later disassembly. At 73 deg F and 50% relative humidity, the typical tack-free time is 1 to 2 hours and the typical cure rate is 4 mm per 24 hours. The sealant can be used with wood, fiberglass, gelcoat, selected plastics, and metals; some plastics require testing and metals may require primer. It is used above and below the waterline on deck-to-hull joints, portholes, deck fittings, rub rails, screw holes, and stanchion supports.

Key features

  • Fast Moisture Cure: Forms a tack-free surface in a typical 1 to 2 hours at 73 deg F and 50% relative humidity.
  • Flexible Disassemblable Seal: The medium-strength elastomeric bond remains flexible and permits later disassembly.
  • Non-Sag Marine Application: The caulkable paste stays non-sagging for marine joints and hardware above or below the waterline.

Applications

Suitable for fiberglass deck-to-hull joints, wood-to-fiberglass bonding, portholes, deck fittings, rub-rail attachment, screw holes, and stanchion supports.

Technical Specifications

General Properties
Color
The color
White, Black
Density (g)
1.2 g/cm3
Solids
100 %
Physical Properties
Tack-Free Time
60 - 120 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
>400 %
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are representative or typical and are not specifications.

PropertyValueUnitMethod / condition
ConsistencyCaulkable, non-sag paste-Typical; as supplied
Density9.75lb/galApproximate; typical
Solids content100%Approximate; typical
Tack-free time1 to 2hoursTypical at 73 deg F (23 deg C) and 50% RH
Rate of cure3/16 (4)in (mm) per 24 hTypical at 73 deg F (23 deg C) and 50% RH
Application surface temperature40 to 100 (4 to 38)deg F (deg C)Do not apply to frost-covered surfaces
Technical properties

Final-state / after-processing properties

Technical values are representative or typical and are not specifications.

PropertyValueUnitMethod / condition
Shore A hardness40-Typical; ASTM C661
Tensile strength180 (1.24)psi (MPa)Typical; ASTM D412
Elongation at break>400%Typical; ASTM D412
Service temperature-40 to 190 (-40 to 88)deg F (deg C)Typical product data