3M 4116

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4116

Main features

  • Fast Initial Multi-Substrate Tack
  • Breathable Contaminant-Trapping Seal
  • High-Density Vibration Damping

Product Description

3M Urethane Foam Tape 4116 is a natural, single-coated, open-cell urethane foam tape with pressure-sensitive acrylic adhesive for cushioning, sealing, and vibration control. Its 1.6 mm (62 mil) firm, high-density foam absorbs vibration and dampens sound while allowing air and gas vapor to pass through. The structure traps moisture, dust, and drafts without creating a closed-cell barrier, and the adhesive provides high initial quick-stick on multiple substrates. Adhesion is typically satisfactory within 20 minutes and continues to build over time. This tape suits electronics cushioning, printers, keyboards, computers, aircraft lights, automotive dashboards, recessed lighting, and door, window, or cabinet seals.

Key features

  • Firm High-Density Cushioning: The urethane foam absorbs vibration and dampens sound in electronic and industrial assemblies.
  • Breathable Open-Cell Sealing: The foam traps moisture, dust, and drafts while allowing air and gas vapor to pass.
  • Fast Initial Acrylic Tack: The pressure-sensitive adhesive provides quick-stick and builds adhesion after application.

Applications

Suitable for electronics cushioning, printers, keyboards, computers, aircraft lights, automotive dashboards, recessed lighting, and door, window, or cabinet seals.

Technical Specifications

General Properties
Color
The color
Natural-white
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
80 %
Other Properties
Storage Temperature
16 - 27 °C
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.066 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
CarrierFirm open-cell urethane foam-As supplied
AdhesiveAcrylic-Pressure-sensitive; one side
ColorNatural-As supplied
Total thickness without liner62 (1.6)mil (mm)As supplied
Density18 (288)lb/ft3 (kg/m3)As supplied
Foam typeFirm, high density-Open cell
LinerSilicone-treated paper-White
Shelf life24monthsProduct classification
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Adhesion buildTypically satisfactory within 20 min-Continues to build with time
BreathabilityAir and gas vapor pass through-Applied open-cell foam
Cushioning and absorbencyExcellent-Applied foam
Sound and vibration responseDampens sound and absorbs vibration-Applied foam
Contaminant controlTraps moisture, dust, and drafts-Applied foam

Leading Brands Trust in Our Products and Services