3M 401M

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 401M

Main features

  • Fast High-Initial Substrate Grab
  • Fast Hand-Tearable Process Handling
  • Defined -40 to 65 deg C Service

Product Description

3M Double Coated Paper Tape 401M is a natural, 9 mil (0.228 mm) double-coated paper tape with rubber-resin pressure-sensitive adhesive for temporary attachment, splicing, and project stabilization. Its soft adhesive develops high initial adhesion and good holding power on a wide range of materials, while the paper carrier adds handling strength and permits hand tearing. The liner improves dimensional stability for die-cutting and automated dispensing and helps control edge roll during processing. After proper room-temperature application, the tape performs from -40 to 150 deg F (-40 to 65 deg C) in long-term service. Applications include splicing paper, foil, film, and fabric, mounting printing plates, attaching golf grips, and temporary part holding.

Key features

  • High-Initial Rubber Adhesion: The soft rubber-resin adhesive provides quick grab and good holding power.
  • Hand-Tearable Paper Carrier: The paper construction adds handling strength and tears by hand during application.
  • Stable Die-Cutting Liner: The densified kraft liner adds dimensional stability and helps reduce edge roll.

Applications

Suitable for splicing and core starting of paper, foil, film, and fabric; printing-plate mounting; golf-grip attachment; and temporary part holding.

Technical Specifications

General Properties
Color
The color
White/Green
Other Properties
Storage Temperature
21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AdhesiveNatural rubber-Pressure-sensitive
CarrierPaper-Double coated
ColorNatural-As supplied
Total thickness without liner9 (0.228)mil (mm)As supplied
Adhesive thickness per side3 (0.08)mil (mm)As supplied
LinerDensified kraft paper-White and green
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Long-term temperature range-40 to 150 (-40 to 65)deg F (deg C)Properly applied tape
Initial adhesionHigh-Room-temperature application
Holding powerGood-Applied tape
Initial bondQuick grab-Pressure-sensitive application

Leading Brands Trust in Our Products and Services