3M 4016

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 4016

Main features

  • High-Shear Permanent Mounting
  • Vibration-Damping Conformable Foam
  • Protected 104 deg C Holding

Product Description

3M Double Coated Urethane Foam Tape 4016 is an off-white, open-cell urethane foam tape with acrylic pressure-sensitive adhesive on both sides for interior mounting and attachment. The 0.0625 in. (1.6 mm) flexible carrier conforms to joined surfaces, dampens vibration, and builds a strong permanent bond. 3M Adhesive 100 provides high ultimate adhesion, high shear holding power, and resistance to elevated temperatures, solvents, chemicals, and environmental exposure. The densified kraft-paper liner supports die-cutting and automated dispensing while limiting edge roll. This tape suits protected interior and exterior mounting, including signs, nameplates, dispensers, acoustic panels, wire clips, and corner protectors.

Key features

  • High-Shear Acrylic Bond: 3M Adhesive 100 develops high ultimate adhesion and very high shear holding power.
  • Conformable Vibration-Damping Foam: The flexible open-cell carrier follows surfaces and dampens vibration in mounted assemblies.
  • Process-Stable Kraft Liner: The densified liner supports die-cutting and automated dispensing while reducing edge roll.

Applications

Suitable for protected mounting of interior signs, nameplates, dispensers, acoustic panels, wire clips, and corner protectors.

Technical Specifications

General Properties
Color
The color
Natural
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
100 %
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
CarrierOpen-cell urethane foam-As supplied
AdhesiveAcrylic-Pressure-sensitive; both sides
ColorOff-white-As supplied
Total thickness without liner59milAs supplied
Nominal product thickness0.0625 (1.6)in (mm)As supplied
Density11lb/ft3As supplied
Liner62 lb densified kraft paper-Green or green plaid
Shelf life24monthsProduct classification
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Elongation at break100%Method not stated
Tensile strength140lb/inMethod not stated
Long-term holding temperatureUp to 220 (104)deg F (deg C)Applied tape
Bond developmentIncreases with natural aging-Applied tape
ResistanceGood temperature and chemical resistance-Applied tape

Leading Brands Trust in Our Products and Services