3M 3747PG

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3747PG

Main features

  • Fast Seconds-Scale Bond Set
  • Moderate 63 deg C Heat Resistance
  • Versatile Plastic-to-Wood Bonding

Product Description

3M Hot Melt Adhesive 3747 PG is a tan, 100% solids thermoplastic hot-melt adhesive in PG stick format for fast industrial assembly with a compatible handheld applicator. Once heated, the adhesive liquefies, wets the bonding surface, and fills gaps before cooling to a strong, tough, flexible bond within seconds. A 50-second open time supports placement and positioning, while moderate heat resistance extends service to 145 deg F (63 deg C). The adhesive bonds many plastics, wood, lightweight metals, fabric, glass, and vinyl for assembly, attachment, repair, panel bonding, wire tacking, bundling, sealing, packaging, and foam-bonding operations. As a thermoplastic, the cured bond can remelt at sufficiently high temperature.

Key features

  • Fast cooling-set behavior: The molten adhesive hardens and develops bond strength within seconds after cooling.
  • Defined positioning window: A 50-second open time supports placement before the hot melt sets.
  • Moderate heat resistance: The cooled bond is rated to 145 deg F (63 deg C).

Applications

Suitable for industrial assembly, attachment, repair, panel bonding, wire tacking, bundling, sealing, packaging, foam bonding, and bonding many plastics, wood, lightweight metals, fabric, glass, and vinyl.

Technical Specifications

General Properties
Color
The color
Tan
Density (g)
0.97 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
265 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
4,100 mPa.s
Chemical Properties
Melting Point
104 °C
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorTan-As supplied
Product formPG stick-Exact configuration
Solids content100%Approximate by weight
Open time50sCondition not stated
Application methodHandheld applicator-Compatible hot-melt equipment
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Heat resistance145 (63)deg F (deg C)Maximum operating value
Shear strength430psiMethod and condition not stated
Bond characterStrong, tough, and flexible-Cooled hot melt
Bond developmentWithin seconds-After application and cooling