3M 363

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 363

Main features

  • High-Tensile Reinforced Foil
  • 316 deg C Continuous Service
  • FAR 25.853(a) Requirements Met

Product Description

3M High Temperature Aluminum Foil/Glass Cloth Tape 363 is a silver, glass-cloth-reinforced aluminum foil tape with a pressure-sensitive silicone adhesive for high-temperature protective wrapping and heat shielding. The flexible 0.19 mm (7.3 mil) laminate follows curved and irregular surfaces while providing high tensile, puncture, fracture, and tear resistance. Its reflective foil supports heat management, and the applied tape performs continuously from -65 to 600 deg F (-54 to 316 deg C). The construction meets FAR 25.853(a) requirements and resists flame, moisture, weather, UV exposure, and chemicals. It is used over insulation, cables, instruments, wire harnesses, and other heat-sensitive components exposed to movement or vibration.

Key features

  • Reinforced flexible laminate: Aluminum foil over glass cloth combines conformability with puncture and tear resistance.
  • Continuous high-temperature service: Applied tape performs from -65 to 600 deg F (-54 to 316 deg C).
  • Defined flame qualification: The exact 363 construction meets FAR 25.853(a) requirements.

Applications

Suitable as heat-reflective wrap over insulation, cables, instruments, wire harnesses, and high-temperature-sensitive components in aerospace and industrial use.

Technical Specifications

General Properties
Color
The color
Silver
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
7 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
236.4 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorSilver-Typical
AdhesiveTransparent silicone-Pressure-sensitive
BackingAluminum foil laminated to glass cloth-As supplied
Glass-cloth thickness0.06 (2.4)mm (mil)Typical; ASTM D3652
Foil thickness0.025 (1)mm (mil)Typical; ASTM D3652
Total tape thickness0.19 (7.3)mm (mil)Typical; ASTM D3652
Shelf life36monthsFrom manufacture; 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

Performance values are typical; methods and conditions are shown in each row.

PropertyValueUnitMethod / condition
180 deg peel adhesion5.7 (52)N/cm (oz/in)Typical; ASTM D3330 at 23 deg C and 304 mm/min
Elongation at break7%Typical; ASTM D3759
Tensile strength236.4 (135)N/cm (lb/in)Typical; ASTM D3759
Long-term temperature range-54 to 316 (-65 to 600)deg C (deg F)Days or weeks