3M 34383

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 34383

Main features

  • Hand-Tearable Foil Installation
  • Vapor-Barrier Sealing Performance
  • Broad -40 to 149 deg C Service

Product Description

3M Aluminum Foil Tape 34383 is a silver, self-wound aluminum foil tape with an aggressive acrylic adhesive for sealing, patching, heat reflection, and vapor-barrier protection. Its 2.8 mil (0.07 mm) high-strength foil backing is malleable enough to follow irregular surfaces and tears by hand for tool-free application. The 4.5 mil (0.11 mm) total construction reflects heat and light and supports durable sealing against moisture, vapor, ultraviolet exposure, and harsh weather. Applied tape has typical peel and tensile data and long-term temperature resistance from -40 to 300 deg F (-40 to 149 deg C), supporting indoor and outdoor holding, splicing, patching, and sealing work.

Key features

  • Malleable foil backing: The high-strength aluminum follows irregular shapes and tears by hand for installation.
  • Vapor-barrier sealing: The foil/acrylic construction provides moisture-vapor protection and waterproof sealing.
  • Broad long-term temperature range: Applied tape is rated from -40 to 300 deg F (-40 to 149 deg C) for days or weeks.

Applications

Suitable for heat reflection and dissipation, repairing tears, splicing thin foils, and general holding, patching, and sealing indoors or outdoors.

Technical Specifications

General Properties
Color
The color
Silver
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
11 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
52.5 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorSilver-Typical
AdhesiveAcrylic-Pressure-sensitive
BackingAluminum foil-As supplied
Backing thickness0.07 (2.8)mm (mil)Typical; ASTM D3652
Total tape thickness0.11 (4.5)mm (mil)Typical; ASTM D3652
Shelf life24monthsFrom manufacture; 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

Performance values are typical; methods and conditions are shown in each row.

PropertyValueUnitMethod / condition
180 deg peel adhesion6.1 (55)N/cm (oz/in)Typical; ASTM D3330 at 23 deg C and 304 mm/min
Elongation at break11%Typical; ASTM D3759
Tensile strength52.5 (30)N/cm (lb/in)Typical; ASTM D3759
Long-term temperature range-40 to 149 (-40 to 300)deg C (deg F)Days or weeks

Leading Brands Trust in Our Products and Services