3M 3302

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 3302

Main features

  • Low-Resistance Conductive Bonding
  • Conformable EMI/RFI Shielding
  • UL 510 Recognized Construction

Product Description

3M Conductive Aluminum Foil Tape 3302 is a silver, dead-soft aluminum foil tape with a conductive pressure-sensitive acrylic adhesive for low-level EMI/RFI shielding and printed-circuit manufacturing or repair. The 2 mil (0.05 mm) high-strength foil is malleable enough to follow irregular and textured surfaces, while the adhesive wets out to low-surface-energy materials and supports a low-resistance conductive bond. The 3.5 mil (0.09 mm) total construction is hand tearable for installation and carries UL 510 recognition. Applied performance includes typical peel and tensile data with long-term temperature resistance from -40 to 250 deg F (-40 to 121 deg C).

Key features

  • Conductive acrylic interface: The adhesive supports low-resistance bonding and electrical continuity across the applied tape.
  • Malleable dead-soft foil: The aluminum backing follows irregular, uneven, and difficult textured surfaces.
  • Wide long-term temperature range: Applied tape is rated from -40 to 250 deg F (-40 to 121 deg C) for days or weeks.

Applications

Suitable for low-level EMI/RFI shielding, printed-circuit manufacturing and repair, grounding, and electrical-continuity applications.

Technical Specifications

General Properties
Color
The color
Silver
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
3 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
33.3 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorSilver-Typical
AdhesiveConductive acrylic-Pressure-sensitive
BackingDead-soft aluminum foil-As supplied
Backing thickness0.05 (2)mm (mil)Typical; ASTM D3652
Total tape thickness0.09 (3.5)mm (mil)Typical; ASTM D3652
Liner thickness0.11 (4.4)mm (mil)Typical
Shelf life12monthsFrom manufacture; 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

Performance values are typical; methods and conditions are shown in each row.

PropertyValueUnitMethod / condition
180 deg peel adhesion2.4 (21)N/cm (oz/in)Typical; ASTM D3330 at 23 deg C and 304 mm/min
Elongation at break3%Typical; ASTM D3759
Tensile strength33.3 (19)N/cm (lb/in)Typical; ASTM D3759
Long-term temperature range-40 to 121 (-40 to 250)deg C (deg F)Days or weeks
RecognitionUL 510-File E230409