3M 30NF

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 30NF

Main features

  • Water-Dispersed Contact Adhesive
  • Heat-Resistant Laminate Bonding
  • Greenguard-Certified Wood and Laminate Bonding

Product Description

3M™ Fastbond™ Contact Adhesive 30-NF is a water-dispersed, sprayable polychloroprene contact adhesive offering a remarkably long bonding range and high coverage. Non-flammable in the wet state, it is engineered to create post-formable, heat-resistant bonds for demanding assembly tasks. This GREENGUARD-certified formulation effectively bonds most foamed plastics, plastic laminate, wood, plywood, and canvas to themselves and to each other.

Key features

  • Water-dispersed formula: Non-flammable in the wet state, improving workplace safety while providing high surface coverage.
  • High performance: Post-formable and highly heat resistant, making it exceptionally effective for decorative laminates and millwork.
  • Low emissions: GREENGUARD certified for low chemical emissions, addressing or contributing to multiple LEED EQ credits.

Applications / Suitable for

  • Bonding foamed plastics, plastic laminate, wood, plywood, and canvas
  • Use with swinging type fire doors of hollow metal and steel composite types
  • Interior building materials requiring low chemical emissions

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Green when wet. Darker green when dry. Neutral, White (Wet), Clear (Dry)
Solids
47 — 51 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-26 °C
Mechanical Properties
Peel Strength
44 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Polychloroprene - -
Color Green (Wet) / Dark Green (Dry) - Also available in Neutral formulation
Solids Content by Weight 47 - 51 % -
Net Weight 8.9 - 9.3 lb/gal (1.06 - 1.11 kg/L)
Viscosity 200 - 750 cP at 27°C (80°F)
Coverage 680 ft²/gal at 3 g/ft² dry
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
180° Peel Adhesion 560 oz/in Canvas to Steel, 72 h at 23°C (73°F)
Overlap Shear Strength 480 lb/in² Birch to Birch at 23°C (73°F)
Overlap Shear Strength 60 lb/in² Birch to Birch at 82°C (180°F)
Flatwise Tensile Strength 113 lb/in² High pressure laminate to particle board at 23°C (73°F)

Leading Brands Trust in Our Products and Services