3M 301

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 301

Main features

  • Clean One-Piece Removal
  • Conformable Paint-Masking Control
  • Defined 107 deg C Exposure

Product Description

3M Performance Yellow Masking Tape 301+ is a yellow crepe-paper tape with a rubber pressure-sensitive adhesive for industrial paint masking. It adheres quickly to metal, rubber, glass, plastic, wood, concrete, and painted surfaces, while the conformable backing follows corners, contours, and irregular shapes. The tape resists paint bleed-through and removes cleanly in one piece without adhesive residue. It withstands surface temperatures up to 225 deg F (107 deg C) for 30 minutes and tears by hand while resisting slivering. This construction suits specialty-vehicle, aerospace, automotive, and general industrial finishing where visible placement and controlled paint edges matter.

Key features

  • Clean one-piece removal: The solvent-free adhesive removes in one piece without adhesive residue.
  • Conformable crepe backing: The high-strength paper follows corners, contours, and irregular surfaces while resisting paint bleed-through.
  • Defined thermal exposure: The tape withstands surface temperatures up to 225 deg F (107 deg C) for 30 minutes.

Applications

Suitable for industrial paint masking, MRO, woodworking, concrete, bundling, color coding, sealing, and mid-temperature paint processes.

Technical Specifications

General Properties
Color
The color
Yellow
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
11 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
35 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BackingCrepe paper-As supplied
AdhesiveRubber-Pressure-sensitive
ColorYellow-As supplied
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Surface-temperature exposureUp to 225 (107)deg F (deg C)30 min
RemovalOne piece; no adhesive residue-Applied tape
Paint barrierResists bleed-through-Most industrial paint systems
ConformabilityCorners, contours, and irregular surfaces-Applied tape