3M 298X

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 298X

Main features

  • Precision Fiber-Protrusion Control
  • Lower Slurry Contamination
  • MT Connector Polishing Fit

Product Description

3M Polishing Film 298X is a pressure-sensitive adhesive-backed, micron-graded aluminum oxide polishing film for water-assisted finishing of MT-style multi-fiber optic connectors and wafer edges. The mineral is coated on a fibrous polyester film backing and is available in nominal 0.5 um pink and 1.0 um light-green grades. During use with water, the film breaks down into a slurry, supporting controlled fiber protrusion and reduced slurry contamination on fixtures and equipment. Its precision construction is intended to improve process throughput and reduce rejects in supported polishing operations where consistent abrasive grade and controlled surface finishing are required.

Key features

  • PSA-backed fibrous film: Micron-graded aluminum oxide is coated on a fibrous polyester backing with pressure-sensitive adhesive.
  • Controlled fiber protrusion: The precision abrasive construction supports better control of protrusion during multi-fiber connector polishing.
  • Water-assisted slurry action: The film breaks down with water to reduce slurry mess and contamination on fixtures and machines.

Applications

Applications include MT-style multi-fiber optic connector polishing and wafer-edge cleaning.

Technical Specifications

General Properties
Color
The color
Pink
Other Properties
Storage Temperature
10 - 30 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Technical data are representative or typical for the explicit 298X grade scope.

PropertyValueUnitMethod / condition
ConstructionAluminum oxide on fibrous polyester film-298X grade
Backing typePressure-sensitive adhesive backed-298X grade
Nominal micron grade and color0.5 pink / 1.0 light greenumTypical; 298X grade
Shelf life24monthsFrom manufacture; original packaging
Storage conditions10 to 30 deg C; 30 to 60% RH-Original packaging