3M 251

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 251

Main features

  • Balanced One-to-One Mixing
  • Defined Oven-Cure Handling
  • Rigid Class F Insulation

Product Description

3M Scotchcast Electrical Resin 251 is a two-part, oven-curing, filled epoxy liquid resin for insulating, potting, filling, and patching electrical and electronic components. Parts A and B mix 1:1 by weight or 50:50 by volume; the mixed resin has typical viscosity of 19,000 cP at 23 deg C and gels in 20 minutes at 121 deg C. The cured rigid Class F system combines 40 Barcol hardness with typical electric strength of 425 V/mil (16.8 kV/mm) on a 1/8 in (3.75 mm) sample. It is used on coils, transformers, motors, modules, and related electrical assemblies requiring physical strength and elevated-temperature electrical performance.

Key features

  • Balanced two-part mixing: Parts A and B mix 1:1 by weight or 50:50 by volume.
  • Defined oven-cure handling: Typical mixed viscosity is 19,000 cP at 23 deg C with 20-minute gel time at 121 deg C.
  • Rigid Class F insulation: The cured filled epoxy provides typical 40 Barcol hardness and 425 V/mil electric strength under the stated conditions.

Applications

Applications include coating, filling, patching, insulating, and potting coils, transformers, motors, modules, and electrical or electronic components.

Technical Specifications

General Properties
Color
The color
Brown
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part (A / B)
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.50
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
0.7 %
Other Properties
Storage Temperature
10 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Component and mixed-material values remain separated, and mix ratios retain their stated basis.

PropertyValueUnitMethod / condition
Mix ratio by weight (A:B)1:1-Before processing
Mix ratio by volume (A:B)50:50%Before processing
Part A viscosity175,000cPTypical at 23 deg C
Part B viscosity10,000cPTypical at 23 deg C
Mixed viscosity19,000cPTypical at 23 deg C
Density (A / B)1.53 / 1.48kg/LTypical
Gel time20minTypical at 121 deg C
Cure guide15 to 20 h / 6 to 8 h / 2 to 3 h-75 deg C / 95 deg C / 120 deg C
Technical properties

Final-state / after-processing properties

Cured properties are typical, not specification limits, and are measured at 23 deg C unless stated otherwise.

PropertyValueUnitMethod / condition
Cured colorBrown-Typical
Hardness40BarcolTypical at 23 deg C
Specific gravity1.50-Typical; cured
Compressive strength17,500psiTypical; 10% compression
Tensile strength5,280psiTypical
Elongation at break0.7%Typical
Electric strength425 (16.8)V/mil (kV/mm)Typical; 1/8 in (3.75 mm) sample
Heat distortion point130 (266)deg C (deg F)Typical; 264 psi