3M 2460

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 2460

Main features

  • Low-Ridge Precision Paint Lines
  • Delicate-Surface Low-Peel Handling
  • Twenty-One-Day Outdoor Removal

Product Description

Scotch Ultimate Paint Edge Masking Tape 2460 is a thin, smooth Washi-paper masking tape with a high-temperature acrylic adhesive for sharp paint edges and low paint ridges. Its 0.08 mm (3.3 mil) construction combines good instant adhesion with low peel force for masking delicate surfaces and protecting finished areas. The tape resists solvent- and latex-based paints, remains removable after exposure up to 300 deg F (149 deg C), and can provide clean outdoor removal from most surfaces for up to 21 days. It is used for straight lines, broad curves, delicate EPDM moldings, and surface protection during industrial finishing and construction.

Key features

  • Thin Washi-paper construction: The 0.08 mm (3.3 mil) backing supports sharp paint lines with a low paint ridge.
  • Low-peel surface protection: Low peel force suits supported delicate-surface masking and protection work.
  • Extended clean removal: The tape supports clean high-temperature removal and outdoor use for up to 21 days on most surfaces.

Applications

Applications include masking straight lines and broad curves, masking delicate surfaces and EPDM moldings, and protecting surfaces from scuffing.

Technical Specifications

General Properties
Color
The color
Yellow
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
6 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
31.5 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Technical values are representative or typical and are not specification limits.

PropertyValueUnitMethod / condition
ColorYellow-Typical
AdhesiveAcrylic-As supplied
BackingSmooth Washi paper-As supplied
Total thickness0.08 (3.3)mm (mil)Typical; ASTM D3652
Tensile strength31.5 (18)N/cm (lb/in)Typical; ASTM D3759
Elongation at break6%Typical; ASTM D3759
Shelf life24monthsFrom manufacture; original packaging at 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
180 deg peel adhesion0.9 (8)N/cm (oz/in)Typical; ASTM D3330 at 23 deg C and 304 mm/min
High-temperature clean removal149 (300)deg C (deg F)Up to 30 min
Outdoor clean-removal periodUp to 21daysMost surfaces
Paint resistanceGood-Solvent- and latex-based paints