3M 232

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 232

Main features

  • Immediate High-Hold Adhesion
  • Clean Medium-Temperature Removal
  • One-Piece Sliver-Resistant Handling

Product Description

3M High Performance Masking Tape 232 is a tan, smooth crepe-paper masking tape for medium-temperature paint bake operations and demanding industrial finishing. Its solvent-free rubber adhesive develops immediate tack on metal, rubber, glass, plastic, and EPDM surfaces, while the heat-resistant backing conforms around corners and irregular shapes. The tape resists lifting, curling, slivering, and adhesive transfer and supports one-piece clean removal under normal operating conditions. On painted panels, it removed cleanly after 30 minutes at temperatures up to 121 deg C, with performance dependent on the surface, paint, processing conditions, and removal temperature. Applications include paint masking, temporary holding, labeling, patching, bundling, and surface protection.

Key features

  • Immediate high-hold adhesion: The rubber adhesive sticks quickly across supported substrates and resists lifting or curling.
  • Clean bake-cycle removal: Painted-panel evaluation showed clean removal after 30 minutes at temperatures up to 121 deg C.
  • One-piece handling: The crepe backing conforms, tears easily, and resists slivering during removal.

Applications

Applications include industrial paint masking, medium-temperature bake masking, temporary holding, labeling, patching, bundling, and surface protection.

Technical Specifications

General Properties
Color
The color
Tan
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
10 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
52.5 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorTan-Typical
BackingSmooth crepe paper-Heat-resistant saturant
AdhesiveRubber-Solvent-free
Total thickness0.16 (6.3)mm (mil)ASTM D3652
Elongation at break10%ASTM D3759
Tensile strength52.5 (30)N/cm (lb/in)ASTM D3759
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
180 deg peel adhesion4.1 (37)N/cm (oz/in)ASTM D3330 at 23 deg C; 304 mm/min
Clean-removal bake resistanceUp to 121 (250)deg C (deg F)30 min on painted panels
ASTM D6123 complianceMeets requirements-Product evaluated; each lot is not tested
Removal behaviorOne-piece; resists slivering-Normal operating conditions

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers