3M 226

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 226

Main features

  • Chemical-Resistant Surface Protection
  • Three-Month Outdoor Clean Removal
  • Quick-Stick Hand-Tearable Handling

Product Description

Scotch Solvent Resistant Masking Tape 226 is a black masking tape with polyethylene film laminated to saturated crepe paper for protection during solvent- and water-based processing. The reinforced backing controls stretch, tears by hand, and resists many solvents, water solutions, emulsions, and selected paint-stripping chemistries. A high-tack natural-rubber adhesive provides quick stick and holding power across metal, plastic, and painted surfaces. The tape removes cleanly from most opaque surfaces for up to three months of outdoor exposure and supports removable use at 107 deg C. Applications include aerospace masking, surface protection, sealing, and hot-air leveling of printed circuit boards.

Key features

  • Chemical-resistant backing: The polyethylene and saturated-crepe construction resists many solvent- and water-based process solutions.
  • Controlled handling: The reinforced backing controls stretch, tears by hand, and supports quick placement.
  • Extended clean removal: The tape removes cleanly from most opaque surfaces for up to three months of outdoor exposure.

Applications

Applications include chemical-resistant masking, sealing and protection of metal, plastic, and painted surfaces, aerospace processing, and hot-air leveling of printed circuit boards.

Technical Specifications

General Properties
Color
The color
Black
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
11 %
Tensile Strength (Thin Film)
Tensile strength determines the resistance of a material to break under tension and it measures how much elongating load (or tensile stress) it can handle before fracture. To make it simple, it measures how much force we have to apply when pulling apart a material before it breaks.
59.5 N/cm
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorBlack-Typical
BackingPolyethylene / saturated crepe paper-Typical
AdhesiveRubber-Typical
Total thickness0.27 (10.6)mm (mil)ASTM D3652
Elongation at break11%ASTM D3759
Tensile strength59.5 (34)N/cm (lb/in)ASTM D3759
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
180 deg peel adhesion4.2 (38)N/cm (oz/in)ASTM D3330 at 23 deg C; 304 mm/min
Removable application temperature107 (225)deg C (deg F)Applied tape
Outdoor clean-removal periodUp to 3monthsMost opaque surfaces
Process-media resistanceMany solvent- and water-based solutions-Applied tape