3M 2216NS

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 2216NS

Main features

  • Flexible Shock/Vibration/Thermal-Cycling Resistance
  • High Peel and Shear Strength
  • Visual Two-Part Mix Confirmation

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray is a flexible, two-part, room-temperature curing epoxy adhesive known for its high peel and shear strength. It offers exceptional resistance to extreme shock, vibration, and flexing, making it ideal for potting parts subject to thermal cycling and cryogenic bonding applications. With its contrasting base and accelerator colors, this structural adhesive ensures a reliable mix and bonds effectively to metals, woods, plastics, rubbers, and masonry products.

Key features

  • Flexible and shock resistant: Absorbs stresses from extreme shock, vibration, flexing, and thermal cycling.
  • High-strength bonding: Delivers excellent shear and peel strength across multiple substrates, retaining performance after environmental aging.
  • Military specification compliant: Meets DOD-A-82720 requirements for high-performance structural applications.

Applications / Suitable for

  • Bonding metals, woods, plastics, rubbers, and masonry
  • Cryogenic bonding applications
  • Potting components subject to thermal cycling

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
2:3
Solids
100 %
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
1.5 hours
Physical Properties
Open time
90 minutes
Viscosity (Part A)
40,000-80,000 mPa.s
Viscosity (Part B)
75,000-150,000 mPa.s
Mechanical Properties
Peel Strength
43.75 N
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.395 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 2:3 - B:A
Mix Ratio by Weight 5:7 - B:A
Color White - Base
Color Gray - Accelerator
Viscosity 75,000-150,000 cP Base at 22°C (72°F)
Viscosity 40,000-80,000 cP Accelerator at 22°C (72°F)
Worklife 90 minutes 100g mixed at 22°C (72°F)
Time to Handling Strength 8-12 hours at 22°C (72°F)
Time to Full Cure 7 days at 22°C (72°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Cured Color Gray - -
Shore Hardness 57 Shore D ASTM D2240 at 22°C (72°F)
T-Peel Adhesion 25 lb/in ASTM D1876 at 22°C (72°F)
Shear Modulus 42 MPa ASTM D1002, tested at 22°C (72°F)
Dielectric Constant 5.51 - ASTM D150, 1 KHz at 22°C (72°F)
Volume Resistivity 1.9E+12 Ohm-cm ASTM D257 at 22°C (72°F)
Total Mass Loss (TML) 0.77 % NASA 1124 Rev 4 at 22°C (72°F)