Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1300L

Main features

  • Brush or Spray Application
  • High Immediate Strength and Heat Resistance
  • Metal, Rubber, and Wood Bonding

Product Description

3M™ Neoprene High Performance Rubber & Gasket Adhesive 1300L is a versatile, polychloroprene-based adhesive designed for bonding rubber and gasket materials. As a lower-solids and lower-viscosity version of 3M Adhesive 1300, it offers easier brushing and sprayability while providing high immediate strength and excellent heat resistance. It effectively bonds neoprene, SBR, and butyl rubber to metal, wood, and most plastics.

Key features

  • Broad temperature resistance: Maintains performance across a wide temperature range from -34°C to 149°C.
  • Fast bonding range: Offers a short bonding range of up to 8 minutes for efficient assembly.
  • Industry compliant: Meets the specification requirements of MMM-A-121.

Applications / Suitable for

  • Bonding neoprene, SBR, and butyl rubber
  • Adhering rubber to metal, wood, and most plastics[
  • General gasket and rubber assembly

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Yellow
Density (g)
part A: 1.00/ part B: 1.15 g/cm3
Solids
26 — 33 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-26 °C
Mechanical Properties
Peel Strength
32 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Polychloroprene - -
Color Yellow - -
Solids Content by Weight 26-33 % -
Viscosity 250-1000 cP at 27°C (80°F)
Flash Point -26 °C Closed Cup
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
180° Peel Adhesion 768 oz/in Canvas to Steel, 72 h at 23°C (73°F)
Overlap Shear Strength 343 lb/in² Birch to Birch, 2 week cure, tested at -34°C (-30°F)
Overlap Shear Strength 549 lb/in² Birch to Birch, 2 week cure, tested at 66°C (150°F)