3M 1300

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1300

Main features

  • Four Minute Dry-To-Touch Time
  • Up to 12-Minute Bonding
  • Rubber-to-Rigid Substrate Bonding

Product Description

3M Neoprene High Performance Rubber and Gasket Adhesive 1300 is a one-part, solvent-based polychloroprene contact adhesive for bonding rubber and gasket materials. It bonds neoprene, reclaimed rubber, SBR, and butyl rubber to metal, wood, and selected plastics. The adhesive reaches a dry-to-touch condition in about four minutes and provides a bonding range up to 12 minutes, allowing positioning before contact assembly. Brush, flow, or spray application can be used for general MRO, rubber gasket attachment, rubber sheeting, and rubber repair; the product is not recommended for EPDM or TPO. Available supply formats include tubes, cans, and bulk packages.

Key features

  • Fast dry-to-touch: A thin uniform coating reaches a dry-to-touch condition in about four minutes.
  • Up to 12-minute bonding: The contact adhesive provides positioning time within a bonding range up to 12 minutes.
  • Defined rubber bonding: The adhesive bonds neoprene, reclaimed rubber, SBR, and butyl to metal, wood, and selected plastics.

Applications

Applications include general MRO, bonding rubber gaskets to metal, attaching rubber to rigid substrates, large-area rubber sheeting, and rubber repair. Do not apply to EPDM or TPO.

Technical Specifications

General Properties
Color
The color
Yellow
Solids
34-39 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-26 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1500-4000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BasePolychloroprene-Typical uncured property
ColorYellow-Typical
Solids content by weight34 to 39%Typical
CarrierPetroleum distillate, methyl ethyl ketone, and toluene-Solvent system
Flash point-26 / -14deg C / deg FClosed cup; typical
Viscosity1500 to 4000cP27 deg C; Brookfield RVF No. 2 spindle at 20 rpm; typical
Bonding rangeUp to 12minAfter dry-to-touch condition; product 1300
Shelf life30monthsFrom manufacture; unopened at 16 to 27 deg C and 40 to 60% RH
Technical properties

Final-state / after-processing properties

Typical peel-adhesion values apply to canvas-to-steel specimens conditioned at 23 deg C.

PropertyValueUnitMethod / condition
180-degree peel adhesion31.5N/cmTypical; canvas to steel, 24 h dwell at 23 deg C
180-degree peel adhesion84.1N/cmTypical; canvas to steel, 72 h dwell at 23 deg C
180-degree peel adhesion89.4N/cmTypical; canvas to steel, 120 h dwell at 23 deg C
180-degree peel adhesion91.1N/cmTypical; canvas to steel, 168 h dwell at 23 deg C

Leading Brands Trust in Our Products and Services