3M 1267

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1267

Main features

  • Embossed Z-Axis Contact
  • 64 dB Average Shielding
  • Lined Die-Cut Handling

Product Description

3M Embossed Aluminum EMI Shielding Tape 1267 uses a 2.0 mil embossed, dead-soft aluminum backing coated with non-conductive acrylic adhesive in a 4.95 mil tape for grounding and EMI control. During installation, raised foil edges penetrate the adhesive and establish z-axis contact with the substrate; conductivity does not come from the adhesive itself. ASTM D4935 testing gives 64 dB average shielding effectiveness across 300 kHz to 2.5 GHz, while the stated MIL-STD-202 method limits electrical resistance to 0.0075 ohm/in2 maximum. A removable liner aids die-cut conversion and controlled placement in equipment, components, shielded rooms, and prototype assemblies.

Key features

  • Embossed contact path: The aluminum embossing penetrates the non-conductive adhesive to establish foil-to-substrate electrical contact.
  • Measured shielding performance: Average shielding effectiveness is 64 dB from 300 kHz to 2.5 GHz under ASTM D4935.
  • Lined die-cut handling: The removable liner supports converting, die cutting, placement, and prototype work.

Applications

Applications include grounding and EMI shielding in equipment, components, and shielded rooms, plus die-cut parts, electrical prototyping, design work, and troubleshooting.

Technical Specifications

General Properties
Adhesive Layer
A layer that is applied to one surface or both to bind items together and resist their separation
non-conductive acrylic
Color
The color
silver
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.051 mm
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
4.96 μm
Mechanical Properties
Adhesion Strength
Adhesion is the bond strength measurement of a coating to a substrate. When an adhesive is bonded to an item or surface, numerous physical, mechanical and chemical forces come into play, which may have an effect on each other.
30.2 Oz/in

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorSilver-Visual
BackingEmbossed aluminum foil-As supplied
AdhesiveNon-conductive acrylic-Non-corrosive pressure-sensitive adhesive
Backing thickness2.0 / 0.051mil / mmNominal
Total thickness4.95 +/- 0.65 / 0.126mil / mmASTM D1000 at 23 deg C
Shelf life5yearsFrom manufacture; 10 to 27 deg C and less than 75% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Electrical resistance0.0075ohm/in2Maximum; MIL-STD-202 Method 307 at 5 psi over 1 in2
Shielding effectiveness64dBAverage; ASTM D4935, 300 kHz to 2.5 GHz at 23 deg C
Adhesion to steel30.2 / 3.3oz/in / N/cmMinimum; ASTM D1000 at 23 deg C
Breaking strength14 / 25lb/in / N/cmMinimum; ASTM D1000 at 23 deg C
Flame retardancyPass-UL 510A, Category OARC2, File E17385