3M 1099

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 1099

Main features

  • Medium-Viscosity Application Control
  • Long-Term Durability by Resisting Weathering
  • Adhesion-Promoting Surface Treatment

Product Description

3M™ Nitrile High Performance Plastic Adhesive 1099 is a fast-drying, medium-viscosity nitrile rubber adhesive designed for brush or flow applications. It cures to form strong, flexible bonds that resist weathering, water, fuels, oil, and plasticizers. This high-performance adhesive can be used at room temperature or heat-cured to obtain superior physical properties, making it highly versatile for various assembly needs.

Key features

  • Fast drying: Rapidly forms strong, flexible bonds to help accelerate production and assembly processes.
  • Exceptional resistance: Delivers robust durability against weathering, water, fuels, oil, and plasticizers.
  • Heat-cure option: May be cured with heat to achieve superior physical and mechanical properties.

Applications / Suitable for

  • Bonding vinyl extrusions and sheeting
  • Adhering fabrics, foams, and many plastics
  • Industrial brush or flow applications

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light Tan
Density (g)
part A: 1.00/ part B: 1.15 g/cm3
Solids
31-37 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-15 °C
Mechanical Properties
Peel Strength
29 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Nitrile Rubber - -
Color Light Tan - Wet and dry
Solids Content by Weight 31-37 % -
Carrier Solvent Acetone - -
Viscosity 2000-4000 cP at 27°C (80°F)
Flash Point -15 °C Closed Cup
Bonding Range Up to 40 minutes -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
180° Peel Adhesion 29 N/cm Canvas to Steel, 24h at 23°C (73°F)
45 N/cm Canvas to Steel, 72 h at 23°C (73°F)
48 N/cm Canvas to Steel, 168 h at 23°C (73°F)
54 N/cm Canvas to Steel, 14 days at 23°C (73°F)
31 N/cm Canvas to Steel, 21 days at -34°C (29°F)
12 N/cm Canvas to Steel, 21 days at 66°C (150°F)
Overlap Shear Strength

3.2 MPa Aluminum to Aluminum, 121°C cure
21 MPa Aluminum to Aluminum, 177°C cure, tested at -55°C
9.0 MPa Aluminum to Aluminum, 177°C cure, tested at 23°C
6.2 MPa Aluminum to Aluminum, 177°C cure, tested at 66°C

Leading Brands Trust in Our Products and Services