3M 08682

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 08682

Main features

  • Automotive Urethane Adhesion Primer
  • Fast-Drying No-Activator Processing
  • UV-Blocking Corrosion-Protection Primer

Product Description

3M™ Single Step Primer 08682 is a one-component polyurethane-based primer designed to promote adhesion between 3M urethane windshield adhesives and automotive glass, primed pinchweld metal, and PVC encapsulated parts. It also functions as a blackout primer to help protect urethane adhesive from ultraviolet exposure while providing corrosion protection for minor pinchweld scratches. The fast-drying formulation requires no activator and is intended for professional automotive glass installation applications. :contentReference[oaicite:0]{index=0}

Key Features

  • One-component primer that promotes adhesion of urethane windshield adhesives to glass, primed metal, and PVC encapsulated parts.
  • Fast drying formulation requiring no activator before use.
  • Blackout primer providing UV protection for urethane adhesives while helping protect minor pinchweld scratches from corrosion.

Applications / Suitable for

  • Automotive windshield replacement
  • Priming automotive glass before urethane bonding
  • Priming PVC encapsulated glass and PAAS windshield systems
  • Touch-up of minor pinchweld scratches
Product Family

3M 08682

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Density (g)
1.0 g/cm3
Solvent
Methyl Ethyl Ketone
Physical Properties
Drying Time
10 minutes
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
50 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Product Form Liquid — As supplied
Color Black — Published property
Dry Time 10 minutes Published property
Viscosity 20 mPa·s 20°C
Shelf Life 9 months Unopened container
Package Size 30 mL PN 08682