3M Single Step Primer 08681 is a black, one-part polyurethane primer for promoting 3M auto glass urethane adhesion to glass, primed pinchweld metal, PVC-encapsulated parts, and PAAS systems. The liquid primer requires no activator and dries for at least 10 minutes at 21 deg C and 50% RH. It also functions as a blackout primer for shielding urethane from ultraviolet exposure and as a touch-up coating for minor bare-metal pinchweld scratches. The product is an application-stage primer within the 3M glass urethane bonding system, not a stand-alone adhesive. The 08681 grade is supplied in a 125 mL aluminum bottle.

Key features

  • One-part primer: The polyurethane primer requires no separate activator and is applied as a uniform coating.
  • Ten-minute drying: The applied primer dries for at least 10 minutes at 21 deg C and 50% RH before urethane bonding.
  • Multiple auto-glass interfaces: The primer is used on automotive glass, primed pinchweld metal, PVC encapsulation, and PAAS systems.

Applications

Applications include priming automotive glass before bonding with 3M auto glass urethane, coating minor bare-metal pinchweld scratches, priming PVC-encapsulated parts, and preparing PAAS windshield systems.

Technical Specifications

General Properties
Color
The color
Black

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
BasePolyurethane resins-Typical
Density1.0g/mLApproximate
ColorBlack-Typical
Viscosity50cPTypical
ConsistencyLiquid-Typical
Drying timeAt least 10min21 deg C and 50% RH
Technical properties

Final-state / after-processing properties

Qualification results apply to the auto-glass urethane bonding system for products 08681 and 08682.

PropertyValueUnitMethod / condition
Initial conditioningPass-72 h at 22 deg C and 50% RH
Water immersionPass-10-day qualification test
Heat agingPass-14 days at 87.8 deg C
Humidity agingPass-14 days at 37.8 deg C and 100% RH
QUV exposurePass-2000 h qualification test