3M 08001

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 08001

Main features

  • Flexible Waterproof Bond
  • Tube-Ready Brush Application
  • Vibration-Resistant Gasket Repairs

Product Description

3M Super Weatherstrip and Gasket Adhesive 08001 is a yellow, one-part solvent-based adhesive for attaching rubber weatherstripping and gaskets to metal. It brushes and spreads directly from the tube, forming a flexible waterproof bond that resists vibration, oils, detergents, solvents, and temperature changes. The adhesive also bonds vinyl, fabrics, rubber, and metal for automotive trim work. Its quick-curing handling profile keeps weatherstripping in place during repairs on doors, trunks, sunroofs, and headliner assemblies, combining direct application with the flexibility needed for components exposed to movement and changing service conditions. The 08001 grade is supplied in a 5 fl oz tube.

Key features

  • Flexible waterproof bond: The cured adhesive holds weatherstripping and gaskets while resisting vibration and water exposure.
  • Direct tube application: The yellow adhesive brushes and spreads from the 5 fl oz tube without separate mixing.
  • Automotive material range: The adhesive bonds rubber, vinyl, fabrics, and metal in supported trim and gasket applications.

Applications

Applications include bonding rubber weatherstripping and gaskets to metal, attaching automotive headliners, and repairing trim on doors, trunks, and sunroofs.

Technical Specifications

General Properties
Color
The color
Yellow
Density (g)
0.91 g/cm3
Solids
39.0 %
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-25.5 °C
Service temperature
-28.89 to 148.89 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
4,500 mPa.s