3M 05096

Main features

  • Fine Small-Defect Filling
  • Smooth Feathered Edges
  • Low-Shrinkage Spot Repair

Product Description

3M Acryl-Green Spot Putty 05096 is a one-component acrylic spot putty for filling minor surface defects before automotive refinishing. The air-drying green material spreads in thin layers and feathers to smooth edges, supporting localized repairs without mixing. Its fast-drying formula is intended for small-area work, and the application thickness must remain 0.16 cm or less. Apply it to clean, sanded, primed surfaces, allow the layer to dry, and sand before priming or top coating. The material is suited to pinholes, sand scratches, stone chips, and other minor blemishes, with controlled spreading, low shrinkage, and smooth edge blending. The 05096 grade is supplied in a 410 g aluminum tube.

Key features

  • Fine defect filling: The single-component acrylic formula fills pinholes, scratches, stone chips, and other minor surface damage.
  • Controlled thin application: The putty is applied in thin layers at a maximum thickness of 0.16 cm.
  • Smooth finishing behavior: Good spreadability, low shrinkage, sanding, and feathering support localized refinishing work.

Applications

Applications include filling pinholes, sand scratches, stone chips, and small surface blemishes on prepared automotive and marine finishes before priming or top coating.

Technical Specifications

General Properties
Color
The color
Green
Density (g)
1.4 – 1.6 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
17.2 °C
Physical Properties
Volatiles
27.6 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ComponentsTalc, acrylic copolymer, toluene-Typical as supplied
Density1.4 to 1.6g/cm3Typical
ColorGreen-Typical
Flash point17.2deg CTypical
Volatile compounds27.6wt%Typical